The wood is cut to size, cleaned through our log cleaner and dropped in to our IBC cages.

The wood can be dried naturally or it can be dried in a kiln.
Our logs are placed in the kiln and the drying process takes 5 days , while the temperature is increased over 70° C and vaporized water is taken out. The kiln is heated only with a hot water in order to avoid fire risks. The hot water is produced by a boiler heated with wood. All our production waste is dried and used for kiln heating.